0.326*1000*C????馬鋼????TDX51D+Z80?2/1?白灰/馬鋼白????6340????菲騰庫
4.92//170601901B????????????????
0.40*1000*C????馬鋼????TDX51D+z120?2/1?白灰(下公差)????6050????
4.91/1665//【501715-10】【2018.3月】【不要噴碼,下公差,基板厚度0.38,臥卷】[馬鞍山政平庫(含出庫費)]????????????????
0.40*1000*C????馬鋼????TDX51D+Z120?2/1?白灰(下公差)????6050????馬鞍山政平庫(含出庫費)
4.865/1654、4.895/1663//【512309-20】【2018.4月】【下公差,基板厚度0.38,臥卷,不需要噴碼】【待付款】????????????????
4.85/1636、4.855/1637、4.865/1640、4.935/1664、4.955/1670//【512309-20】【2018.4月】【下公差,基板厚度0.38,臥卷,不需要噴碼】【暫未入庫】????????????????
0.40*1000*C????馬鋼????TDX51D+z120?2/1?海藍(下公差)????6140????菲騰庫
3.92/1333//【463542-20】【2017.9月】【要噴碼下公差,基板厚度0.38mm】????????????????
0.40*1000*C????馬鋼????TDX51D+z120?2/1?海藍(下公差)????6140????菲騰庫
4.865/1649//【489616-10】【2018.1月】【下公差,基板厚度0.38mm,臥式包裝,要有噴碼】????????????????
0.40*1000*C????馬鋼????TDX51D+Z120?2/1?鐵青灰(下公差)????6290????
3.19/1078、3.125/1056、3.12/1055、//【496651-10】【18.2月】【背面必須有馬鋼噴碼,下公差,基板厚度0.38mm,臥式包裝】[菲騰庫]????????????????
4.185/1413、4.295/1450//【496651-10】【18.2月】【背面必須有馬鋼噴碼,下公差,基板厚度0.38mm,臥式包裝】[菲騰庫]????????????????
0.40*1000*C????馬鋼????TDX51D+Z120?2/1?鐵青灰(下公差)????6200????馬鞍山政平庫(含出庫費)
(4.435/1514、4.86/1658、4.96/1695、4.68/1589、4.825/1636、3.52/1195、4.23/1441、3.665/1230待付款)//【512309-110】【18.4月】【下公差,基板厚度0.38,臥卷,不需要噴碼】????????????????
0.40*1200*C????馬鋼????TDX51D+Z120??2/1?白灰正品????5740????菲騰庫
1.2//171211961B????????????????
0.40*1200*C????馬鋼????TDX51D+Z120??2/1?白灰(下公差)????6140????西浜1號庫
2.245/617//【201610-13】[396348-10]????????????????
0.40*1200*C????馬鋼????TDX51D?白灰(下公差)????6140????上海興晟庫
4.85/1373//【416951-20】【17.2月】????????????????
0.4*1200*C????馬鋼????TDX51D+Z120?2/1?白灰(下公差)????6140????菲騰庫
3.435/971//【463761-30】【17.9月】【不噴碼,下公差,基板厚度0.38mm】????????????????
0.4*1200*C????馬鋼????TDX51D+Z120?2/1?白灰(下公差)????6050????馬鞍山政平庫(含出庫費)-文兆庫(共悅路355號)入上海中岐實業有限公司
3.355/952、5/1414//【491271-10】【18.1月】【合格品,2/1,PE,白灰,背面馬鋼白?Z120,下公差,臥式包裝,要有噴碼,現充期】????????????????
0.40*1200*C????馬鋼????TDX51D+Z120?2/1?白灰(下公差)????6050????
3.505/988//【512309-30】【2018.4月】【下公差,基板厚度0.38,臥卷,不需要噴碼】[馬鞍山政平庫(含出庫費)-文兆庫(共悅路355號)入上海中岐實業有限公司]????????????????
4.225/1195、4.225/1194、4.39/1243、4.37/1237、4.19/1185、4.205/1189、4.205/1189、//【512309-30】【2018.4月】【下公差,基板厚度0.38,臥卷,不需要噴碼】【暫未入庫】[馬鞍山政平庫(含出庫費)]????????????????
0.40*1200*C????馬鋼????TDX51D?海藍(下公差)????6140????菲騰庫
3.4/962、//【17.2月】【416389-20】????????????????
0.40*1200*C????馬鋼????TDX51D+Z120?2/1?海藍(下公差)????6140????菲騰庫
4.12/1151//【17.7月】【451259-60】【背面不要馬鋼噴碼,下公差,基板厚度0.38mm】????????????????
0.40*1200*C????馬鋼????TDX51D+Z120?2/1?海藍(下公差)????6140????菲騰庫
3.99/1132、3.99/1132、////【17.8月】【455748-130】【合格品,2/1,PE,Z120,不噴碼,下公差,基板厚度0.38mm】????????????????
0.40*1200*C????馬鋼????TDX51D+Z120?2/1?海藍(下公差)????6140????菲騰庫
4.955/1406、4.99/1413//【17.11月】【478575-20】【背面必須有馬鋼噴碼,下公差,基板厚度0.38mm,臥式包裝】????????????????
0.40*1200*C????馬鋼????TDX51D+Z120?2/1?海藍(下公差)????6050????馬鞍山政平庫(含出庫費)
4.595/1303、3.43/952、3.315/921、3.315/921、3.3/920、3.285/921、4.86/1381、3.395/945//【18.2月】【496638-20】【背面有馬鋼噴碼,下公差,基板厚度0.38mm,臥式包裝】????????????????
0.40*1200*C????馬鋼????TDX51D+Z120?2/1?鐵青灰/鋼白(下公差)????6290????菲騰庫
4.87/1374、4.825/1363//【17.9月】【464835-10】【背面不需馬鋼噴碼,下公差,基板厚度0.38mm】????????????????
0.40*1200*C????馬鋼????TDX51D+Z120?2/1?鐵青灰/鋼白(下公差)????6290//6200????
4.97/1403、4.8/1353、//【17.9月】【463542-30】【要噴碼下公差,基板厚度0.38mm】【菲騰庫】????????????????
4.66/1312、4.56/1282、4.615/1300、4.485/1263、4.475/1262、4.825/1360、4.835/1363//【17.9月】【463542-30】【要噴碼下公差,基板厚度0.38mm】【馬鞍山政平庫(含出庫費)】????????????????
0.40*1200*C????馬鋼????TDX51D+Z120?2/1?緋紅????5990????菲騰庫
2.09/557//170600641B????????????????
0.45*1000*C????馬鋼????TDX51D+Z120?2/1?白灰(下公差)????5900????馬鞍山政平庫(含出庫費)
4.855/1461、4.84/1447、3.08/929、3.96/1191、//【512309-40】【2018.4月】【下公差,基板厚度0.43,臥卷,不需要噴碼】????????????????
0.45*1000*C????馬鋼????TDX51D+Z120?2/1?銀色(金屬)(下公差)????6090????菲騰庫
4.915/1476//【496064-10】【2018.1月】【背面必須有馬鋼噴碼,下公差,基板厚度0.43mm,臥式包裝】????????????????
0.45*1000*C????馬鋼????TDX51D+Z120?鐵青灰(下公差)????6140????菲騰庫
4.935/1466//【454883-10】【17.7月】【背面不需馬鋼噴碼,下公差,基板厚度0.43mm】????????????????
0.45*1000*C????馬鋼????TDX51D+Z120?鐵青灰(下公差)????6140????菲騰庫
4.84/1462、//【483754-10】【17.12月】【背面必須有馬鋼噴碼,下公差,基板厚度0.43mm,臥式包裝】????????????????
0.45*1000*C????馬鋼????TDX51D+Z120?銀灰(非金屬)(下公差)????6090//6000????
4.025/1205、4.25/1273、4.06/1212、//【496638-40】【18.2月】【背面必須有馬鋼噴碼,下公差,基板厚度0.43mm,臥式包裝】【菲騰庫】????????????????
4.255/1273、4.675/1398、4.83/1443//【496638-40】【18.2月】【背面必須有馬鋼噴碼,下公差,基板厚度0.43mm,臥式包裝】【馬鞍山政平庫(含出庫費)】????????????????
0.45*1000*C????馬鋼????TDX51D+Z120?2/1?馬鋼中灰(7016)?????6190????菲騰庫
4.94//160806642B????????????????
0.45*1200*C????馬鋼????TDX51D+Z120?2/1?白灰????5890????菲騰庫
2.085//160804704B????????????????
0.45*1200*C????馬鋼????TDX51D+Z120?2/1?白灰????5990????上海浦達庫(聯誼路398 T:66037703 F:66030721)
?【4.76//160700582B????4.815//160801712B?嚴重變形】??【已在BS名下】????????????????
3.78//160700602B?????4.85//160700571B????4.95//160801701B?????????4.935//160801711B?????4.715//160801722B?????4.815//160801812B??????4.745//160801821B【已在BS名下】????????????????
4.64//160801763B???4.775//160801782B???4.395//160801783B????4.945//160801791B????4.795//160801792B????4.735//160801801B???4.725//160801802B????4.42//160801803B?????4.9//160801811B【已在BS名下】????????????????
0.45*1200*C????馬鋼????TDX51D+Z120?2/1?海藍(下公差)????5990????上海興晟庫
2.585/649、2.76/693//【443167-30】【17.6月】【背面無馬鋼噴碼下公差,基板厚度0.43mm】????????????????
0.45*1200*C????馬鋼????TDX51D+Z120?2/1?海藍(下公差)????5990????上海興晟庫
4.935/1226、4.925/1222//【445604-30】【17.6月】【背面無馬鋼噴碼下公差,基板厚度0.43mm】????????????????
0.45*1200*C????馬鋼????TDX51D+Z120?2/1?海藍????5990????菲騰庫
3.47//170602783B??????3.55//170602782B????3.54//170602781B??????4.995//170602792B????????????????
0.45*1200*C????馬鋼????TDX51D+Z120?2/1?海藍(下公差)????5900????馬鞍山政平庫(含出庫費)
4.02/1010、4.085/1024、4.095/1024、3.77/945、3.855/966//【447785-50】【17.7月】【不噴碼,下公差,基板厚度0.43mm】????????????????
0.45*1200*C????馬鋼????TDX51D+Z120?2/1?海藍(下公差)????5900????馬鞍山政平庫(含出庫費)
4.595/1152、4.595/1151、4.615/1161//【464835-50】【17.9月】【背面不需馬鋼噴碼,下公差,基板厚度0.43mm】????????????????
0.45*1200*C????馬鋼????TDX51D+Z120??2/1?鐵青灰【正品】????5840????菲騰庫
1.89//180300814B???????1.735//180300813B?????????????????
0.45*1200*C????馬鋼????TDX51D+Z120?2/1?鐵青灰/鋼白(下公差)????6140????菲騰庫
4.715/1180、4.53/1133//【496638-120】【18.2月】【背面不要馬鋼噴碼,下公差,基板厚度0.43mm,臥式包裝】????????????????
0.50*1000*C????馬鋼????TDX51D+Z120?2/1?海藍(下公差)????5740????菲騰庫
4.53/1217、//【511357-10】【2018.4月】【下公差,基板厚度0.48mm,不需要噴碼】????????????????
0.50*1000*C????馬鋼????TDX51D+AZ100?鍍鋁鋅海藍(下公差)????5890????上海興晟庫1
4.63/1245、4.765/1281、4.765/1280、//【428208-20】?【17.4月】【有噴碼?】????????????????
0.50*1000*C????馬鋼????TDX51D+Z120?2/1?瓷藍(下公差)????5840//5750????
4.87/1309、4.88/1312、4.78/1284、//【509528-40】【2018.4月】【下公差,基板厚度0.48,臥卷,不需要噴碼】【菲騰庫】
馬鋼彩鋼卷,馬鋼彩涂板,馬鋼氟碳板,馬鋼鍍鋁鋅彩涂板,馬鋼聚酯彩板,馬鋼彩涂卷
馬鋼彩涂板使用環境對板材的影響
一、自然環境的影響(不同地區)
不同地區彩涂鋼板的選擇主要考慮的是當地的風雪載荷以及腐蝕環境。風雪載荷主要是考慮建筑物的安全系數,這盡管和彩涂鋼板的力學性能有關,但更多的和壓型鋼板的板形、厚度以及板與板之間的連接有關。而定量描述一個地區的腐蝕環境相對困難,影響彩涂鋼板的腐蝕因素有很多。如:溫度、濕度、晝夜溫差、日照時間和日照強度、降雨量和降雨的酸度、風向和風速、腐蝕性沉降物等。
馬鋼彩涂鋼板抗腐蝕影響的要素
它們分別為涂料種類、涂料厚度、涂料供應商、鍍層種類、鍍層厚度、預處理種類、鋼板厚度、涂層結構等。
馬鋼彩涂板施工設計對腐蝕的影響
安裝或加工質量:它主要體現在加工時涂層是否損壞,是否在低溫下涂層脆性時加工,安裝時拖動鋼板導致損傷,安裝時結構焊接鐵屑掉落在涂層上,施工完畢不對屋面板進行清掃等,這樣都會引起材料的腐蝕。
從上面這么多對彩涂鋼板腐蝕因素的介紹,以及我們用戶使用情況反饋和暴曬試驗結果分析,我們對不同地區的使用建議如下:
在紫外線強烈的高原(西南和西北)和低緯度地區(廣東及以南地區)考慮彩涂鋼板應該選擇耐久性優越的涂層(PVDF涂層、HDP涂層、SMP涂層等),在高溫高濕地區(南方沿海大部分地方)涂層及鍍層都要選擇耐腐蝕優越的材料,鍍層厚度和涂層厚度至少要達到國家標準要求。
在海邊使用彩涂鋼板,需要厚涂層的彩涂鋼板或者涂層相對致密的涂料品種,因為海水中的氯離子滲透能力很強,它能透過薄涂層或者不致密的涂層直接腐蝕基體鍍層,當然,基板必須是鍍鋅或鍍鋁鋅材料。在海水能濺到的地方,不建議采用彩涂鋼板。
工業性環境中,對彩涂的影響主要是酸雨,這些區域集中在湖南、重慶、江西等一帶,聯系采用高鋅層鍍鋅基板的彩涂,彩涂層還是要求厚而致密。在其他不屬于上述地區,用彩涂鋼板的選擇余地就比較大,只要符合彩涂國家標準就可以了。
二、使用環境的影響(不同行業)
不同行業對彩涂鋼板的使用分兩方面來分析,其一就是彩涂鋼板的外板,正常情況下就按不同地區選擇就行了,但也要考慮小環境的影響,即是否在附近有腐蝕介質落到廠房圍護結構上,如燒鍋爐排放的氣體、二氧化硫灰塵等,這在設計時應該考慮煙囪的高度和當地的主要風向等。另外,還有就是廠房密封性如何,也有可能廠房內高溫高濕
帶腐蝕性的氣體冒出來在室外遇冷空氣從而在彩涂鋼板上結露,這種現象要避免,它會加速局部腐蝕的產生;其二是考慮彩涂鋼板的內板(雙層復合鋼板)或背面漆(單層板)。這里要說明的就是相對來說屋面內板比墻面內板更容易腐蝕,如果工人能在該環境下工作,使用彩涂鋼板是可以的。但室內環境的好壞或環保裝置的投入會直接影響
馬鋼彩涂鋼板的使用壽命。
有色金屬冶煉廠(銅、鋅、鋁、鉛等)是較挑戰彩涂鋼板使用年限的。但是合理的選擇材料、設計、以及環保投入等能保證或提高彩涂鋼板的使用壽命。10年進行更換或維護是能做到的。鋼鐵廠、發電廠等也會產生腐蝕性的介質,但彩涂鋼板都有長時間使用的經驗。
機械制造業(汽車、汽輪機、機床等)基本上不會對彩涂腐蝕帶來負面影響,但要注意這些行業可能有熱處理爐、鍋爐等也會影響到局部環境,處理不好會帶來彩涂鋼板的腐蝕,尤其在加工損傷處或切邊處。
倉儲物流這個行業發展較快,使用輕鋼也較多,本身不對彩涂板產生腐蝕,它對彩涂鋼板的選擇主要考慮大環境的影響,一般這樣的工程都集中在工業發達及交通繁忙的地方,也就是工業環境以及沿海地區。
公用及民用建筑美觀、經久耐用是彩涂鋼板首要考慮的因素。因此,涂層抗變色、抗粉化以及涂層表面完整細膩就相當重要。公用及民用建筑關注的人多,且近距離,因此,涂料選擇一般采用PVDF或HDP,并且多選擇淺顏色。

彩涂板,業內又稱彩鋼板,彩板。彩色涂層鋼板是以冷軋鋼板和鍍鋅鋼板為基板,經過表面預處理(脫脂、清洗、化學轉化處理),以連續的方法涂上涂料(輥涂法),經過烘烤和冷卻而制成的產品。

彩鋼板應用比較廣泛。具有無污染、優秀的耐候性、抗腐蝕、高加工等特性。彩鋼板廣泛應用于建筑、家電、運輸、包裝、機械加工、室內裝修、醫療、汽車工業等。

常見的二涂二烘型連續彩色涂層機組工藝流程主要生產工序為:開卷機-------縫合機------壓輥------漲力機----開卷活套-----堿洗脫脂------清洗----烘干-------鈍化-------烘干------初涂-------初涂烘干------面漆精涂------面漆烘干------風冷降溫------收卷活套-----收卷機-----(下卷打包入庫)。